EASYARC 308L
Description
Technical Parameter
Model EASYARC 308L
Conformance AWS A5.4/ASME SFA 5.4:E308L- 17GB 983: E308L-17
Welding Position 1G
2G
2F
3G
4G
Diameters/Packaging (mm) 2.5x300
3.2x350
4.0x350
5.0x350
All Weld Metal Mechanical Properties – TYPICAL
- AWS E308L-17 Required
Tensile Strength (MPA) ≥520
Elongation (%) ≥ 35 - GB E308L-17 Required
Tensile Strength (MPA) ≥520
Elongation (%) ≥ 35 - EASYARC™ 308L
Tensile Strength (MPA) 635
Elongation (%) 49.5
All Weld Metal Chemical Compositions (WT-%) – TYPICAL
- AWS E308L-17 Required
C ≤0.04
Cr 18.0-21.0
Ni 9.0-11.0
Mo ≤0.75
Mn 0.5-2.5
Si ≤1.00
P ≤0.04
S ≤0.03 - GB E308L-17 Required
C ≤0.04
Cr 18.0-21.0
Ni 9.0-11.0
Mo ≤0.75
Mn 0.5-2.5
Si ≤1.00
P ≤0.04
S ≤0.03 - EASYARC™ 308L
C 0.02
Cr 20.14
Ni 9.21
Mo 0.061
Mn 0.71
Si 0.85
P 0.023
S 0.009
FN 6-10
Recommended Welding Current (Current Polarity: DC+ & AC)
- Welding Position: 1G,2G,2F
2.5x300: 50-85
3.2x350: 80-120
4.0x350: 100-150
5.0x350: 140-180 - Welding Position: 3G up, 4G
2.5x300: 45-80
3.2x350: 70-110
4.0x350: 90-140 - *Application: 18%Cr-8%Ni Austenitic stainless steel ASTM 304, 304L, 0Cr18Ni9 or equivalent Steels
*For electrodes that had a short or mild exposure to the atmosphere then re-drying at 300®C for 1 hour will be sufficient. For electrodes that have been exposed to longer or more aggressive conditions or for critical work redrying at 300-350®C for 1-2 hours is recommended. After redrying electrodes should be stored in a hot box.